Ultramid A3ZG7 OSI BK23273
PA66-I-GF35BASFA3ZG7 OSI BK23273 03/2026 PA66-I-GF35 BASF Corporation 33% glass reinforced, heat stabilized, impact modified PA66 black with a combination of excellent impact resistance, toughness and strength.
물성치 데이터
Typical values for uncoloured product at 23°C
| 물성 항목 | 시험 방법 | 단위 | 건조 (Dry) | 조습 (Cond.) |
|---|---|---|---|---|
| properties | ||||
| Polymer abbreviation | - | - | PA66-I-GF35 | |
| Density | ISO 1183 | kg/m³ | 1350 | |
| processing | ||||
| Molding shrinkage (parallel) | ISO 294-4 | % | 0.20 | |
| Molding shrinkage (normal) | ISO 294-4 | % | 0.90 | |
| mechanical | ||||
| Tensile modulus | ISO 527-1/-2 | MPa | 9340 | - |
| Stress at break | ISO 527-1/-2 | MPa | 147 | - |
| Strain at break | ISO 527-1/-2 | % | 4.9 | - |
| Charpy unnotched impact strength (23°C) | ISO 179/1eU | kJ/m² | 115 | - |
| Charpy unnotched impact strength (-30°C) | ISO 179/1eU | kJ/m² | 117 | - |
| Charpy notched impact strength (23°C) | ISO 179/1eA | kJ/m² | 35 | - |
| Charpy notched impact strength (-30°C) | ISO 179/1eA | kJ/m² | 21 | - |
| thermal | ||||
| Deflection temp. under load 1.8 MPa (HDT A) | ISO 75-1/-2 | °C | 246 | |
| Deflection temp. under load 0.45 MPa (HDT B) | ISO 75-1/-2 | °C | 259 | |
기술 자료
관련 PA66-I-GF35 Grade
Glass fiber reinforced injection moulding grade with high stiffness, very good flowability, and excellent heat ageing resistance up to at least 220 °C for technical articles.
Glass fibre reinforced injection moulding grade with good resistance to hydrolysis, suited for processing by water injection technology (WIT). Applications in the automotive cooling circuit, e.g. cooling water pipes.
Glass fibre reinforced injection moulding grade with good resistance to hydrolysis. I.e.: for applications in automotive cooling circuit. This product can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties do not change.
Glass fibre reinforced and heat aging resistance injection moulding grade for industrial articles having very high rigidity.
Glass fibre reinforced and heat aging resistance injection moulding grade for industrial articles having very high rigidity. Material models for crash simulation with Ultrasim™ are available.
Glass fibre reinforced injection moulding grade with optimised heat ageing performance for industrial articles having very high rigidity.